By fgayford - 12/2/2012 2:49:30 PM				
            
                      
            Hi guys
  I have been cutting and trimming Carbon with the following.
  Dremel Tool    -   Jigsaw with a carbid grit blade    -    4 inch cut off wheel -  Vibrator Tool -  Chisel
  I am about to make a Carbon Fiber Violin of a Strad 1701 copy that I just bought for that purpose.
  If you have ever looked at the F holes you can see the problems of the fine cuts involved.
  What would be the best way? A 3d water jet would probably be the best, but real expensive.
  Have you guys had any experience where real fine perfect cuts are involved?
  Or could a steady hand with a dremel also get me there. Perhaps used like a router with a template guide.
  Which cutters are the best?   Carbid   Diamond .
  Thanks
  Fred
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By fgayford - 12/3/2012 2:46:44 AM				
            
                      
            Thanks Guys, seems like the router and good bits are the way to go and finishing up with needle files.
  Fred
           
		 | 			
		 
	
	
						
		 	
		
	 |