Group: Forum Members
Posts: 237,
Visits: 4.8K
|
The car shown is painted with house of kolour polyurethane candy and a gloss lacquer on top. Halando,not as simple as you think If you use a tinted lacquer all your eggs are in one basket so to speak,doing it separately you can get the right amount of colour on to make the carbon " pop" as little or as much as you want . Then your lacquer for your depth an shine
|