Hanaldo - 1/2/2020 8:34:54 AM
You can construct it in the normal way, but then you need to coat the inside with an especially high chemically resistant epoxy, regular epoxy won't do. You need a Phenol Novolac epoxy. Look for epoxy tank sealers, and just make sure they are a two part product, the single part tank sealers are no good.

Thank you very much for your help.
I will look for it....

Hanaldo
Hanaldo
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
You can construct it in the normal way, but then you need to coat the inside with an especially high chemically resistant epoxy, regular epoxy won't do. You need a Phenol Novolac epoxy. Look for epoxy tank sealers, and just make sure they are a two part product, the single part tank sealers are no good.
Nuno_Silva
N
Supreme Being (92 reputation)Supreme Being (92 reputation)Supreme Being (92 reputation)Supreme Being (92 reputation)Supreme Being (92 reputation)Supreme Being (92 reputation)Supreme Being (92 reputation)Supreme Being (92 reputation)Supreme Being (92 reputation)
Group: Forum Members
Posts: 6, Visits: 47
Hey There,
I intend to make a  Motorcycle Fuel tank in Carbon Fiber by infusion creating probably a 6 part mold.
My question is, how can i "glue" 6 parts and how can i insulate inner side for gasoline use.
Does  Epoxy resin will be good or do i have to cover inside tank with something?
Thanks..



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search