+xYou can construct it in the normal way, but then you need to coat the inside with an especially high chemically resistant epoxy, regular epoxy won't do. You need a Phenol Novolac epoxy. Look for epoxy tank sealers, and just make sure they are a two part product, the single part tank sealers are no good.
Thank you very much for your help.
I will look for it....