wayne livesey
wayne livesey
posted 7 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 27
Hi I have made many river tables now with this same method but in this translucent black I have a problem. I have a line in the resin that follows the shape of my live edge the resin is rock solid it's been on my router sled so it's not a surface problem either the top of the table has the problem but the bottom is very dark like the pigment has dropped to the bottom in places. It's 100% mixed properly and never had anything like this happen before and to follow a uniform line on the live edge I no somethings up but have no clue what it's was done in two pours at 20mm each I need an answer for this it's driven me crazy all week
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Translucent pigment problem
wayne livesey
-
7 Years Ago
Is that mark on the surface? does it sand out? It looks like it could be where the pigments sunk a bit and there is some refraction there. or it could be where it has sunk/separated it has left a bit...
Warren (Staff)
-
7 Years Ago
No it's not on the surface it's been on my router sled and sanded it's all the way through the resin it won't polish out I've tried it's a shame there really is not that much pigment in there it look...
wayne livesey
-
7 Years Ago
You could sand way a couple of mm of the resin then backfill with properly pigmented resin to hide it? That may be a way to recover it. I would certainly go for solid colour pigments on future table...
Warren (Staff)
-
7 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search