By wayne livesey - 11/27/2019 10:58:49 PM				
            
                      
            Hi I have made many river tables now with this same method but in this translucent black I have a problem. I have a line in the resin that follows the shape of my live edge the resin is rock solid it's been on my router sled so it's not a surface problem either the top of the table has the problem but the bottom is very dark  like the pigment has dropped to the bottom in places. It's 100% mixed properly and never had anything like this happen before and to follow a uniform line on the live edge I no somethings up but have no clue what it's was done in two pours at 20mm each I need an answer for this it's driven me crazy all week 
      
  
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By Warren (Staff) - 11/28/2019 5:04:06 PM				
            
                      
            You could sand way a couple of mm of the resin then backfill with properly pigmented resin to hide it?  That may be a way to recover it.