How to clean S120 coated moulds?


Author
Message
moonpie
moonpie
Supreme Being (420 reputation)Supreme Being (420 reputation)Supreme Being (420 reputation)Supreme Being (420 reputation)Supreme Being (420 reputation)Supreme Being (420 reputation)Supreme Being (420 reputation)Supreme Being (420 reputation)Supreme Being (420 reputation)
Group: Forum Members
Posts: 34, Visits: 94
I have a mould that has been coated with S120 to leave a nice glossy finish. Thanks to another problem I now have lots of raw infusion resin on the mould surface. Can I clean this off with acetone or easy composites mould cleaner without damaging the S120 surface coating? If not, is there anything I can clean the in2 resin off with and leave the S120 surface intact? Any experiences gratefully received, thanks.