How to clean S120 coated moulds?


Author
Message
moonpie
moonpie
Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)
Group: Forum Members
Posts: 34, Visits: 94
I have a mould that has been coated with S120 to leave a nice glossy finish. Thanks to another problem I now have lots of raw infusion resin on the mould surface. Can I clean this off with acetone or easy composites mould cleaner without damaging the S120 surface coating? If not, is there anything I can clean the in2 resin off with and leave the S120 surface intact? Any experiences gratefully received, thanks.
Reply
Lester Populaire
L
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
moonpie - 11/13/2019 10:37:57 AM
I have a mould that has been coated with S120 to leave a nice glossy finish. Thanks to another problem I now have lots of raw infusion resin on the mould surface. Can I clean this off with acetone or easy composites mould cleaner without damaging the S120 surface coating? If not, is there anything I can clean the in2 resin off with and leave the S120 surface intact? Any experiences gratefully received, thanks.

Cured resin is pretty inert and solvents won't do anything. Assuming you have applied release agent the traces should come off with scotch tape that you rub on so it sticks nicely,  or with just a bit of compressed air.