How to clean S120 coated moulds?


Author
Message
moonpie
moonpie
Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)
Group: Forum Members
Posts: 34, Visits: 94
I have a mould that has been coated with S120 to leave a nice glossy finish. Thanks to another problem I now have lots of raw infusion resin on the mould surface. Can I clean this off with acetone or easy composites mould cleaner without damaging the S120 surface coating? If not, is there anything I can clean the in2 resin off with and leave the S120 surface intact? Any experiences gratefully received, thanks.
Replies
Lester Populaire
L
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
moonpie - 11/14/2019 6:54:11 PM
Thanks Lester but it's not cured resin it's raw resin without hardener, so the question still stands, can i clean this off with acetone without damaging the S120?

How did you manage to do that? 

moonpie
moonpie
Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)
Group: Forum Members
Posts: 34, Visits: 94
Lester Populaire - 11/14/2019 10:26:59 PM
moonpie - 11/14/2019 6:54:11 PM
Thanks Lester but it's not cured resin it's raw resin without hardener, so the question still stands, can i clean this off with acetone without damaging the S120?

How did you manage to do that? 

Hardener past it's shelf life unfortunately...big mess!