	Group: Forum Members 	        
    Posts: 34, 
    Visits: 94 
    
 
          
		     | 
				                       
                 
                
                    
			            I have a mould that has been coated with S120 to leave a nice glossy finish. Thanks to another problem I now have lots of raw infusion resin on the mould surface. Can I clean this off with acetone or easy composites mould cleaner without damaging the S120 surface coating? If not, is there anything I can clean the in2 resin off with and leave the S120 surface intact? Any experiences gratefully received, thanks.                
			            				
			                                 
                     
                                            
                         
                    
                  
             |