Ok.made my first ever part (sheet) from CF.I'm not concern about small imperfections.on the surface cos finally still can be sanded down and 2k clear coat. I more worry about how to remove trapped air. 
Is it degassing ? 
Should I vacuum during infiusion till air stop coming out?
Or anything else?