alternative (cheaper) material to practise resin infusion
alternative (cheaper) material to practise resin infusion
Post Reply
Like
3
alternative (cheaper) material to practise resin infusion
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
8900120d
8900120d
posted 7 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 37,
Visits: 939
can 2x2 woven fibreglass be used to practise infusion instead of carbon fibre?
im new to this and have wasted a load of carbon fibre.
would there be any drawbacks in using woven fibreglass instead?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
alternative (cheaper) material to practise resin infusion
8900120d
-
7 Years Ago
Absolutely. No real drawbacks, it's exactly the same in terms of the infusion process. In fact it can even be beneficial as the fibreglass will turn transparent and allow you to see any voids...
Hanaldo
-
7 Years Ago
If its just for practice then yes, glass fibre for sure and you could also consider using a polyester infusion resin rather than epoxy to also bring the costs down - the parts won't be as strong so i...
Rich (Staff)
-
7 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search