By 8900120d - 7/14/2019 6:11:14 PM
can 2x2 woven fibreglass be used to practise infusion instead of carbon fibre? im new to this and have wasted a load of carbon fibre. would there be any drawbacks in using woven fibreglass instead?
|
By Rich (Staff) - 7/16/2019 10:56:48 AM
If its just for practice then yes, glass fibre for sure and you could also consider using a polyester infusion resin rather than epoxy to also bring the costs down - the parts won't be as strong so if you did want to use them in the future for any reason, you may want to add a couple of extra layers to increase the thickness and strength.
|
|