Group: Administrators
Posts: 167,
Visits: 4.6K
|
If its just for practice then yes, glass fibre for sure and you could also consider using a polyester infusion resin rather than epoxy to also bring the costs down - the parts won't be as strong so if you did want to use them in the future for any reason, you may want to add a couple of extra layers to increase the thickness and strength.
|