Rob5
R
Rob5
posted 6 Years Ago
ANSWER
HOT
Topic Details
R
Group: Forum Members
Posts: 1,
Visits: 14
What would be recommended for gluing an aluminium fork expander / sleeve in a carbon fork tube on a road bike. It would be subjected to vibration from riding on road etc.
Reply
Like
3
Warren (Staff)
Warren (Staff)
posted 6 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
With the high levels of vibration, I would look at our
ET515 Semi Flexible 15min Professional Epoxy Adhesive
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
3
Rich (Staff)
Rich (Staff)
posted 6 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 167,
Visits: 4.6K
Although given the nature of the fixing, you would find that VM100 would work as well; it has good flexural properties and the etching property is likely to be advantageous. I don't think you'd go wrong with either of the above.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search