By Rob5 - 2/27/2019 5:33:07 PM

What would be recommended for gluing an aluminium fork expander / sleeve in a carbon fork tube on a road bike. It would be subjected to vibration from riding on road etc.
By Rich (Staff) - 3/1/2019 4:01:32 PM

Although given the nature of the fixing, you would find that VM100 would work as well; it has good flexural properties and the etching property is likely to be advantageous. I don't think you'd go wrong with either of the above.