What would be recommended for gluing an aluminium fork expander / sleeve in a carbon fork tube on a road bike. It would be subjected to vibration from riding on road etc.
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
With the high levels of vibration, I would look at our ET515 Semi Flexible 15min Professional Epoxy Adhesive


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Rich (Staff)
Rich (Staff)
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Administrators
Posts: 167, Visits: 4.6K
Although given the nature of the fixing, you would find that VM100 would work as well; it has good flexural properties and the etching property is likely to be advantageous. I don't think you'd go wrong with either of the above.