I need to make a cf bonnet, but only one piece(the outside one). The inside part (reinforcement) is not to be made.
What is your opinion about the layers to be used?
1 - 2 cf layer 200grs - soric 2mm - 2 cf layer 200grs
2 - 2 cf layer 200grs - soric 2mm - 1 cf layer 650grs
Or another one different?