Hello,

I need to make a cf bonnet, but only one piece(the outside one). The inside part (reinforcement) is not to be made.

What is your opinion about the layers to be used?

1 - 2 cf layer 200grs - soric 2mm - 2 cf layer 200grs 

2 - 2 cf layer 200grs - soric 2mm - 1 cf layer 650grs

Or another one different? 

Thanks,

Pedro
By pedcrist - 10/30/2012 1:49:04 PM

Ok, i´m cleared.