Hi all,

Im trying the new XC110 prepregs but i seem to get no nice results at all. with other (cheaper) prepregs i get really nice and smooth surfaces.
Here is what the parts look like. The oven was set at the values from the curing data sheet. im using thin mould from tooling gelcoat and epoxy/fiberglass.
The tempsensor was laying on the mould itself. should i try increasing more heat at the soak from 4 hours at 70 degrees?