Hi all,

Im trying the new XC110 prepregs but i seem to get no nice results at all. with other (cheaper) prepregs i get really nice and smooth surfaces.
Here is what the parts look like. The oven was set at the values from the curing data sheet. im using thin mould from tooling gelcoat and epoxy/fiberglass.
The tempsensor was laying on the mould itself. should i try increasing more heat at the soak from 4 hours at 70 degrees?







Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
That looks like our EG60 Tooling gelcoat which with a post cure is only rated to 80C at best.  Certainly the 120C section of the cure will be pushing what it is capable of which may explain the matt finish. 


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search