Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Looks like there is a bit of bridging that wont be helping. I would try moving the temperature probe for a start, I've never ever had good results with the probe sitting on the part.
What tooling gelcoat are you using??
|