Steve Broad
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 408,
Visits: 4.1K
Am I doing it wrong? When laying up prepreg my gloves (from EC) stick so much to the carbon that I end up taking them off. It is particularly bad if heat is used when persuading the stuff into shape.
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Gloves sticking to prepreg
Steve Broad
-
8 Years Ago
No, fairly normal. Probably a bit too warm in your work environment, if you can regulate the temperature to about 20 degrees then that's typically when pre-pregs are at their optimum tack. From...
Hanaldo
-
8 Years Ago
Normally hardly touch the material apart from picking up Flick the backing off with a blade tip an loosely position 99% of the work then is done with my "dibber" Highly technical composite term there...
f1rob
-
8 Years Ago
Hi Rob Yes, I am. That would be great, thanks. If you drop me a line at stephenpbroad@aol.com I will send you my contact details and address. Steve
Steve Broad
-
8 Years Ago
after a while you end up with a draw full like this !
f1rob
-
8 Years Ago
my main weapons of choice Can laminate virtually anything with these two !!
f1rob
-
8 Years Ago
rob you wouldn't believe it but some of the 'experts' i work with are looking at starting a company making dibbers :)
scottracing
-
8 Years Ago
That will be cos they can't make anything good in carbon 😁 Better copyright my designs PDQ !!!
f1rob
-
8 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search