Gloves sticking to prepreg


Author
Message
Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Am I doing it wrong? When laying up prepreg my gloves (from EC) stick so much to the carbon that I end up taking them off. It is particularly bad if heat is used when persuading the stuff into shape. 
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
No, fairly normal. Probably a bit too warm in your work environment, if you can regulate the temperature to about 20 degrees then that's typically when pre-pregs are at their optimum tack. From memory, the EC gloves are also quite thin. You can get thicker gloves that are more robust and make it a bit easier. 

Its otherwise just part of working with pre-preg, you get used to it. You can leave the blue backing film on as you get the ply mostly into place and then peel it off just before you press it firmly down. Just make sure not to get any film stuck between plies. I also like to keep a piece of scrunched up backing film and using that to press things into place.

Edited 7 Years Ago by Hanaldo
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search