By Steve Broad - 10/25/2018 8:45:47 AM
Am I doing it wrong? When laying up prepreg my gloves (from EC) stick so much to the carbon that I end up taking them off. It is particularly bad if heat is used when persuading the stuff into shape.
|
By f1rob - 10/27/2018 7:36:08 PM
That will be cos they can't make anything good in carbon 😁 Better copyright my designs PDQ !!!
|
|