resin infusing on a two part mold
resin infusing on a two part mold
Post Reply
Like
10
resin infusing on a two part mold
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
tha_pop
tha_pop
posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 17,
Visits: 877
Hi guys, i have two part mold and i now need to make part from this mold and i was wondering how i can infuse using the two part mold such that the resin will not leak, has anyone come across this issue, any suggestions will be greatly appreciated.
Thanks.
Reply
Like
10
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
resin infusing on a two part mold
tha_pop
-
14 Years Ago
I have also been considering this, have you tried it yet? From what I have collected you use a bit...
Carbon Tuner
-
14 Years Ago
yes i have, i'm using a 3 piece mould. use silicone sealant and bolt the pieces together, after use...
neilb
-
14 Years Ago
Cool thanks, I'd love to see a pic of a 3 part mold!
Carbon Tuner
-
14 Years Ago
I did a couple of two part molds and infused them. I had made a groove in the joining flanges and...
fgayford
-
14 Years Ago
Hello Tha PoP, May this picture help your project,...
Leon
-
14 Years Ago
It depends on the size of the mold but you can envelope bag without leaking
NikCFC
-
14 Years Ago
[quote][b]NikCFC (14/11/2012)[/b][hr]It depends on the size of the mold but you can envelope bag...
andygtt
-
14 Years Ago
Im still amazed how you managed to do such a complex mould and get such good results with very...
Warren
-
14 Years Ago
Post Reply
Like
10
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search