			            yes i have, i'm using a 3 piece mould. use silicone sealant and bolt the pieces together, after use just rub off the silicone sealer, job done!
  i would say that when your getting ready to start laying up your mould, if you make some small balls of wax then cut them in half and stick them on your flanges, when you come to do the other side remove the wax and continue as normal. in doing this on a straight flanged edge you get locating dimples so your mould is always correctly aligned                
			            				
			                                 
                     
                                            
                         
                    
                  
             |