resin infusing on a two part mold


Author
Message
tha_pop
tha_pop
Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)Supreme Being (127 reputation)
Group: Forum Members
Posts: 17, Visits: 877
Hi guys, i have two part mold and i now need to make part from this mold and i was wondering how i can infuse using the two part mold such that the resin will not leak, has anyone come across this issue, any suggestions will be greatly appreciated.

Thanks.
Reply
neilb
neilb
Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)
Group: Forum Members
Posts: 107, Visits: 504
yes i have, i'm using a 3 piece mould. use silicone sealant and bolt the pieces together, after use just rub off the silicone sealer, job done!

i would say that when your getting ready to start laying up your mould, if you make some small balls of wax then cut them in half and stick them on your flanges, when you come to do the other side remove the wax and continue as normal. in doing this on a straight flanged edge you get locating dimples so your mould is always correctly aligned
Edited 13 Years Ago by neilb