bakero
b
bakero
posted 8 Years Ago
ANSWER
HOT
Topic Details
b
Group: Forum Members
Posts: 1,
Visits: 13
Hello,
May I use GlassCast3 on the top of GlassCast 10/50 to have a flat coating?
Best ragards
Peter
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
GlassCast3 on the top of GlassCast 10/50
bakero
-
8 Years Ago
Yes you can. It is commonly done in the way you describe for exactly the reason of a smoother floor. You can either pour the GlassCast 3 when the previous resin layer has cured to the firm but tacky....
Warren (Staff)
-
8 Years Ago
Hi, Is 3 much harder than 10, I'm sure I read it's good for counter tops etc? many thanks, Paul
Paul88
-
8 Years Ago
The hardness is pretty similar. The use of GlassCast 3 on top of 50 is primarily done for the surface smoothness and hence the ability to pour it without further finishing.
Warren (Staff)
-
8 Years Ago
Great cheers Warren. It's definitely a lot harder now, just ordered a load of fine papers to get it to a nice finish! Thanks for your help.
Paul88
-
8 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search