Hello,

May I use GlassCast3 on the top of GlassCast 10/50 to have a flat coating?

Best ragards
Peter

Reply
Paul88
P
Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)
Group: Forum Members
Posts: 4, Visits: 12
Warren (Staff) - 7/30/2018 8:17:49 AM
Yes you can.  It is commonly done in the way you describe for exactly the reason of a smoother floor.  You can either pour the GlassCast 3 when the previous resin layer has cured to the firm but tacky stage or if you wait until it has gone hard, you will need to sand the surface and clean before pouring.

Hi,

Is 3 much harder than 10, I'm sure I read it's good for counter tops etc?

many thanks,

Paul

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search