Hello,
I want to make a bicycle frame by prepreg vacuum bagging process . I am going to use foam as a mold.
I am looking for a foam to withstand the temperature that the prepreg needs to cure.
what type of foam do you suggest?
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
hadi1990 - 8 Years Ago
oekmont - 8 Years Ago
Warren (Staff) - 8 Years Ago
hadi1990 - 8 Years Ago
oekmont - 8 Years Ago
SleepingAwake - 8 Years Ago
hadi1990 - 8 Years Ago
oekmont - 8 Years Ago
Fasta - 8 Years Ago
hadi1990 - 8 Years Ago
Hanaldo - 8 Years Ago
hadi1990 - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search