By hadi1990 - 5/11/2018 5:42:15 AM
Hello, I want to make a bicycle frame by prepreg vacuum bagging process . I am going to use foam as a mold. I am looking for a foam to withstand the temperature that the prepreg needs to cure. what type of foam do you suggest?
|
By hadi1990 - 8/18/2018 10:33:05 PM
Hi,
I am going to make a Styrofoam mold, but after cutting the foam into the final shape, since the structure is so thin (9mm thickness) i'm afraid it's gonna break wrapping the layers over it. can i coat the surface of the Styrofoam with gelcoat or Glasscast to make it stronger?
|
|