I want to make a bicycle frame by prepreg vacuum bagging process . I am going to use foam as a mold.
I am looking for a foam to withstand the temperature that the prepreg needs to cure.
what type of foam do you suggest?
Reply
hadi1990
h
Supreme Being (207 reputation)Supreme Being (207 reputation)Supreme Being (207 reputation)Supreme Being (207 reputation)Supreme Being (207 reputation)Supreme Being (207 reputation)Supreme Being (207 reputation)Supreme Being (207 reputation)Supreme Being (207 reputation)
Group: Forum Members
Posts: 15, Visits: 651
Thank you for the replies,

could you please give some more information about the tube to tube process?
is it like making all the parts seperately and connecting them togheter after curing?
but how about making a mould for tube to tube process? what material do you suggest for mould making?
( i don't have the equipment and machines to do negative moulding)

thanksSmile
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
hadi1990 - 7 Years Ago
oekmont - 7 Years Ago
Warren (Staff) - 7 Years Ago
hadi1990 - 7 Years Ago
oekmont - 7 Years Ago
SleepingAwake - 7 Years Ago
hadi1990 - 7 Years Ago
oekmont - 7 Years Ago
Fasta - 7 Years Ago
hadi1990 - 7 Years Ago
Hanaldo - 7 Years Ago
hadi1990 - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search