Dear All, I need to manufacture thick plates in Carbon fiber composite, 80 mm thickness, 40 mm width, 380 mm length. I would like to make them by hand layup, taking care of work by layers to avoid the exothermy bend or twist the plates. I am right?. Those plates will be then mechanized to make a kind of banana shape. I have epoxy lamination resin, so could I use it?
Attached are two pictures. 1.jpg is the final shape to obtain assembling the mechanized pieces, and 2.jpg is the profile to obtain once mechanized the thick plate.


your suggestions are welcome!

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Dessert Mix - 8 Years Ago
Hanaldo - 8 Years Ago
scottracing - 8 Years Ago
Dessert Mix - 8 Years Ago
scottracing - 8 Years Ago
Dessert Mix - 8 Years Ago
oekmont - 8 Years Ago
Dessert Mix - 8 Years Ago
oekmont - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search