We use PCB cutter bits which seem to work very well.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
adzpz
adzpz
Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)
Group: Forum Members
Posts: 5, Visits: 33
Thanks Warren. Do you know where I could source a 1/4" carbide router bit for cutting carbon fibre sheet?

Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
For something so small, I would say cover over then drill out once a couole of layers if resin have cured.  You should then get a nice crisp edge that you can shape and sand if needs be for a perfect fit.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
adzpz
adzpz
Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)
Group: Forum Members
Posts: 5, Visits: 33
I have a piece of aluminium which is about 3mm thick, I wish to carbon skin on both sides (front and back). 
The piece has two M6 holes in it which I need to retain once skinned.

How do skin around these holes?
Is it best to skin over the holes and then drill them out once cured or should I try and skin around / through them whilst laying up?