By adzpz - 12/18/2017 12:03:22 PM
I have a piece of aluminium which is about 3mm thick, I wish to carbon skin on both sides (front and back). The piece has two M6 holes in it which I need to retain once skinned.
How do skin around these holes? Is it best to skin over the holes and then drill them out once cured or should I try and skin around / through them whilst laying up?
|
By Warren (Staff) - 12/18/2017 12:32:01 PM
We use PCB cutter bits which seem to work very well.
|
|