Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Carbon skinning whilst retaining holes?
Carbon skinning whilst retaining holes?
Post Reply
Like
6
Carbon skinning whilst retaining holes?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Warren (Staff)
Warren (Staff)
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
We use PCB cutter bits which seem to work very well.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
7
adzpz
adzpz
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 5,
Visits: 33
Thanks Warren. Do you know where I could source a 1/4" carbide router bit for cutting carbon fibre sheet?
Reply
Like
6
Warren (Staff)
Warren (Staff)
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
For something so small, I would say cover over then drill out once a couole of layers if resin have cured. You should then get a nice crisp edge that you can shape and sand if needs be for a perfect fit.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Tags
fixings
holes
sandy.
Skinning
Reply
Like
6
adzpz
adzpz
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 5,
Visits: 33
I have a piece of aluminium which is about 3mm thick, I wish to carbon skin on both sides (front and back).
The piece has two M6 holes in it which I need to retain once skinned.
How do skin around these holes?
Is it best to skin over the holes and then drill them out once cured or should I try and skin around / through them whilst laying up?
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search