The amount of epoxy that 2mm soric needs ??? please HELP
The amount of epoxy that 2mm soric needs ??? please HELP
Post Reply
Like
3
The amount of epoxy that 2mm soric needs ??? please HELP
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
abdulhazem
a
abdulhazem
posted 9 Years Ago
ANSWER
HOT
Topic Details
a
Group: Forum Members
Posts: 5,
Visits: 37
I wants to purchase the 2mm lantor soric that easy composites has. I have read on the specification sheet that it takes 1 kg of epoxy per 1 meter square is that correct, because i feel that it is too much !!
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
The amount of epoxy that 2mm soric needs ??? please HELP
abdulhazem
-
9 Years Ago
Those figures are correct. There is quite a lot of gaps between the soric that fill with resin. If you run the infusion resin rich, it can be even more. However it is not all bad as the resin...
Warren (Staff)
-
9 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search