Those figures are correct.  There is quite a lot of gaps between the soric that fill with resin.  If you run the infusion resin rich, it can be even more.

However it is not all bad as the resin honeycomb matrix adds to the strength of the panel as well as the core still being much lighter than a similar solid laminate thus saving weight for a panel of similar stiffness made from solid material.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
abdulhazem
a
Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)
Group: Forum Members
Posts: 5, Visits: 37
I wants to purchase the 2mm lantor soric that easy composites has. I have read on the specification sheet that it takes 1 kg of epoxy per 1 meter square is that correct, because i feel that it is too much !! 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search