Group: Forum Members
Posts: 550,
Visits: 27K
|
Also, peel ply on the whole part would be an good idea, as long as you can't put down the vacuum bag without pleats. The resin will flow in every little corner, and will leave your part with a thousand "resin razor edges" on the back. I have some nice little scars from this on my fingers. I do a lot of infusions, and a good amount of the with soric, but I allways use peel ply and flow mesh all over the part.
|