By andy47 - 9/5/2017 9:35:28 AM
I want to use 2mm Lantor Soric for building a model boat and I want to place the infusion spiral in the middle of the part. Do I need to cut the Lantor Soric in halves just below the infusion spiral or will the resin flow through it? On all videos I have seen, the resin starts flowing from the edge, but I am not sure if I can put the spiral on top.
|
By Warren (Staff) - 4/5/2018 9:05:57 AM
Nice video. Glad it worked out well for you.
|
|