Hi All,


A friend just phoned me abut helping with making a carbon bonnet for a race car from an old mould suited for wet-laying.

He's plan is to wax the mould, clear gel coat it then wet lay the carbon in a general purpose polyester laminating resin, (same as the previous layup).

The bonnet is going to be wrapped so the finish is not important.


Is GC50 only compatible with epoxy resins?


What would be the best Clear Gel Coat for a polyester laminating resin ...



I'm normally an infusion guy and never really use a gel-coat, just clear coat.


Cheers,


Davro





David Stevens
YouTubeComment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search