Hi Davro ..
He would not need to use GC50 ... if he's just going polyester all the way, he can just use a clear Polyester gelcoat -- it would be just like laying up a "normal" glassfibre job.
He might want to experiment a bit with a back layer of black tinted polyester if he only lays down one layer of Carbon, and backs up with Glass
"Sapere Aude"... Dare to KNOW!