Hi All,


A friend just phoned me abut helping with making a carbon bonnet for a race car from an old mould suited for wet-laying.

He's plan is to wax the mould, clear gel coat it then wet lay the carbon in a general purpose polyester laminating resin, (same as the previous layup).

The bonnet is going to be wrapped so the finish is not important.


Is GC50 only compatible with epoxy resins?


What would be the best Clear Gel Coat for a polyester laminating resin ...



I'm normally an infusion guy and never really use a gel-coat, just clear coat.


Cheers,


Davro





David Stevens
YouTubeComment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Hi Davro ..


He would not need to use GC50 ... if he's just going polyester all the way, he can just use a clear Polyester gelcoat -- it would be just like laying up a "normal" glassfibre job.

He might want to experiment a bit with a back layer of black tinted polyester if he only lays down one layer of Carbon, and backs up with Glass

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
We would very strongly advise against trying to use GC50 with a polyester resin.  The GC50 has been uniquely formulated to be epoxy compatible in its cured surface finish by being tack free (as well as the formulation).  If you tried to use a polyester resin on the back of a cured GC50, assuming there was no reaction of one against the other, you would find the gelcoat would delaminate very badly, ruining the part.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search