Group: Forum Members
Posts: 15,
Visits: 28
|
I have always wanted to make carbon fiber running boards for my truck. I don't want to spend $640 US on step boards that are too close to the cab that when you step out, you only touch the outer part. I would much rather spend $650 and make my own from carbon. The stock design is oval, but I want to make them the way I want them to look. I want a 6" wide with 2" of depth. They will be 80" long. Would two C shaped pieces work best and then bond them together OR does anyone have any other ideas?
Mike
|