Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Projects
»
Motorsport, Vehicle Design and Modification
»
Two piece part (running boards) options ****INPUT PLEASE*****
Two piece part (running boards) options ****INPUT PLEASE*****
Post Reply
Like
2
Two piece part (running boards) options ****INPUT PLEASE*****
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
mwr2452
mwr2452
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 15,
Visits: 28
OK, that got me thinking. If I looked at it as if it were a bonnet- outer top layer(s) and then a grid like support skeleton with mounting fixtures laid in...........
Reply
Like
2
mwr2452
mwr2452
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 15,
Visits: 28
2" built out of carbon and core materials is a good idea. If I went that route, maybe only 1 inch thick would do?
Reply
Like
3
Carbon Tuner
Carbon Tuner
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 104,
Visits: 422
Well I bet it would be a cheap durable solution to just go with the tubular style running boards, but they would be black
checkout this stuff:
https://www.easycomposites.co.uk/roll-wrapped-carbon-fibre-tube
Also yes if you were slick enough you could make 2 molds to make a top and bottom for the 6x 2 plank layout. Or maybe just make one mold and fill it with core materials to get 2" thick? I have 0 experience with core materials but someone may chime in if 2" is possible with core materials. Its gonna need to be strong so thick core may be in order.
If Brute Force Isn''''t working your not using enough...
Reply
Like
3
mwr2452
mwr2452
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 15,
Visits: 28
I have always wanted to make carbon fiber running boards for my truck. I don't want to spend $640 US on step boards that are too close to the cab that when you step out, you only touch the outer part. I would much rather spend $650 and make my own from carbon.
The stock design is oval, but I want to make them the way I want them to look. I want a 6" wide with 2" of depth. They will be 80" long.
Would two C shaped pieces work best and then bond them together OR does anyone have any other ideas?
Mike
Attachments
mynewtruck.jpg
(
602 views,
49.00 KB
)
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search