miengreenvega
miengreenvega
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 8,
Visits: 128
Hello, I am just starting out making a carbon fiber front end for a 1965 El Camino and want to start by making the mold for the hood and wonder if lacquer primer would be good enough finnish if it would polish good enough to help prevent the mold from sticking to harshly or what would be the best coating to use? Thank You...
Reply
Like
2
Fasta
Fasta
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 3.5K
Some primers work and some can stick really bad. Primers are after all designed for good adhesion to the top coats.
It's certainly a nice way to go when you can just sand a primer nice and smooth or even polish it a bit, then polish your mould further when done.
But you should just do your own small test sample with the primer and exact release system/technique etc to know for sure if it releases ok.
Fastacraft Facebook page
Reply
Like
2
Hanaldo
Hanaldo
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Most polyester primers will work, some polyurethane primers will work. If you're using a regular automotive or any other polyurethane primer, ALWAYS test it! Better to test any new products if you haven't used them before.
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search