By miengreenvega - 12/12/2016 1:09:55 AM

Hello, I am just starting out making a carbon fiber front end for a 1965 El Camino and want to start by making the mold for the hood and wonder if lacquer primer would be good enough finnish if it would polish good enough to help prevent the mold from sticking to harshly or what would be the best coating to use? Thank You...
By Hanaldo - 12/12/2016 2:20:05 AM

Most polyester primers will work, some polyurethane primers will work. If you're using a regular automotive or any other polyurethane primer, ALWAYS test it! Better to test any new products if you haven't used them before.