Hello, I am just starting out making a carbon fiber front end for a 1965 El Camino and want to start by making the mold for the hood and wonder if lacquer primer would be good enough finnish if it would polish good enough to help prevent the mold from sticking to harshly or what would be the best coating to use? Thank You...
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
Some primers work and some can stick really bad. Primers are after all designed for good adhesion to the top coats.

It's certainly a nice way to go when you can just sand a primer nice and smooth or even polish it a bit, then polish your mould further when done.

But you should just do your own small test sample with the primer and exact release system/technique etc to know for sure if it releases ok.




Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Most polyester primers will work, some polyurethane primers will work. If you're using a regular automotive or any other polyurethane primer, ALWAYS test it! Better to test any new products if you haven't used them before.
 