Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Kinetic,

Just picking up on this thread, had this issue been resolved. The Xencast P6 is our pride and joy at the moment having been a long time in development so I want to make sure we resolve any issues customers are having. Generally the feedback has been amazing.

What type of silicone are you casting into? Addition Cure or Condensation Cure? - What brand; our or someone else's?

Kind regards, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Sparky2305
Sparky2305
Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)
Group: Forum Members
Posts: 10, Visits: 69
Hi Warren

 Silicone mold, aluminium trihydroxide filler, weight, well shaken and de-gassed. The same process we have been using with your previous resin system but with very different results unfortunately.

Thanks 


Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Hi Kinetic,

What type of fillers are you using? and what type of mould did you use? It is very unusual for Fast Cast Polyurethanes to not go off unless something has gone very very wrong.

Was the resin measured out by weight? Also was Part A shaken so redistribute any settled sediment?

We have not heard of any problems with our Fast Cast resin, in fact I made a couple of small casts last night with no issues, so I am keen to try and work out what has gone wrong. So any information you can give would be useful to resolve the problem.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Sparky2305
Sparky2305
Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)
Group: Forum Members
Posts: 10, Visits: 69
Hi

 Has anyone used the new Xencast P6 resin yet? I'm struggling with it as I type I have a part that has been curing for over an hour at 20 degrees plus as the mold was warm and the part is still green. I have mixed the same amount of fillers and pigment as I used to with the old system but the results with xencast seem terrible in comparison.

 Like to hear anyone's experiences with it.

Thanks 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search